Dulon lacquer is nearly the only option for do it yourself painting, but is very very old technology. It is an emulsion-based system that relies on solvent evaporation to form the paint layer.
Newer 2K (2 pack) paints are isocyanate based paints with as it says, two chemical components (actually many chemical components, but two parts to the polymer system). Isocyanates react with the correct second component to make polyurethane polymers, which forms the paint.
These paints MUST be painted with a positive air-feed breathing system as isocyanates are highly toxic and carcinogenic. ie they will poison you.
They must also be heat treated after applying inorder for the polymerisation to occur.
They are also more flexible and resiliant than Dulon types of paint which need a plasticiser to be added for fairings otherwise the paint will crack very easily.
If you use Dulon, do not use Plastikote primer and then Dulon top coat. The Dulon will not adhere well to the plastikote primer unless you use a tack cloth. But that can be difficult to do without screwing up the finish.
Enjoy.
"Life is what happens to you while you're busy making other plans." John Ono Lennon.
"If you have never stared off into the distance then your life is a shame." Counting Crows
"The girls were in tight dresses, just like sweets in cellophane" Joe Jackson
Bookmarks